Hollow glass production process
Jun 23, 2022
Leave a message
The heated glass should be gradually pressed to the required thickness using multiple sets of rollers. Each group of pressure rollers should be parallel to each other to ensure uniform thickness of pressed glass.
The temperature of the adhesive strip at the outlet of the press should be controlled between 40-55 ℃.
The sealing operation of the insulating glass with 3 composite adhesive strips is completed through a three-step process of pressing, bending, and pinching.
① Pressing: Squeeze the outer adhesive strip along the vertical direction of the edge towards another section of the adhesive strip until the two sections of the adhesive strip completely blend together;
② Turn: Smooth the excess glue along the space layer in the middle of the insulating glass, so that there is no excess glue on the outside;
③ Pinch: Pinch two pieces of glass inward to eliminate the gap caused by the separation of the glass outward due to pressure and bending.